Manufacturing and study the structural and electrical properties of the compounds Pb (Zr, Ti)O3 prepared in a manner Powders
Main Article Content
Abstract
Was prepared lead Zrconat titanate compounds with the chemical formula Pb (Zr1-x Tix) O3 as (x = 0.5,0.48) and using technology the way powders were prepared Plasticizer models at a temperature (1000˚C) and for (6hr). physical tests of the models were conducted, where it was the study of the structural properties, in terms of X-ray diffraction measurements as results showed that all models were four-wheel installation (Tetragonal) with Miller transactions (001), (100), (110), (111), (002), (200), (210), (211), (220), (221), (103) and that the prevailing trend is (110) and the results of plasticity microwave very close sense of distance intra-convergent also relatively few crystalline defects. Increasing the bulk density of the true density of altered concentration of zirconium and titanium. Results of the examination microscope-mail also showed that the particle size (Dnm) be tight between the models and the homogeneity of the granules, as well as increasing the homogeneity of compositional structure, causing an improvement in the physical properties and A mechanical. shown technique results EDAX compound of the interacting elements of the composition and there is little difference between the real weight and the weight is noticeable. To study the electrical properties as included electrical properties study both the dielectric constant true of both types ('ε) and fantasy ("ε) as well as the loss of the separation (tanδ) and connectivity alternating (σac)
Article Details

This work is licensed under a Creative Commons Attribution 4.0 International License.
Tikrit Journal of Pure Science is licensed under the Creative Commons Attribution 4.0 International License, which allows users to copy, create extracts, abstracts, and new works from the article, alter and revise the article, and make commercial use of the article (including reuse and/or resale of the article by commercial entities), provided the user gives appropriate credit (with a link to the formal publication through the relevant DOI), provides a link to the license, indicates if changes were made, and the licensor is not represented as endorsing the use made of the work. The authors hold the copyright for their published work on the Tikrit J. Pure Sci. website, while Tikrit J. Pure Sci. is responsible for appreciate citation of their work, which is released under CC-BY-4.0, enabling the unrestricted use, distribution, and reproduction of an article in any medium, provided that the original work is properly cited.
References
1. D.meyer hofer, Transition to the ferroelectric state in barium titanate, physical review.112, 2,11,58 .
2. Damjanovic D,S cience of Hysteresis ,ed. G Bertotti and I. Mayergoyz, Elsevier, 76 241 (1987).
3. A. Ballato , IEEE T. Ultrason. Ferr. 42 916 (1965) .
5. B.D. Cullity "Introduction to Magnetic Materials", Wesley, Mas achusetts , U.S.A , (1972) .
6. Annual Book of ASTM Standards 13 , 180-182, (1979).
7. Paul Barnes, T.C., Simon Jacques Advanced Certificate in Powder Diffraction on the Web. Bragg's Law, (2006).
8. P. Mitra, Khan, "Materials chemistry and physics", (2008) 986.
9. S. Kumar and R. Chandra: Temperature dependent studies of CdS nanoparticles in viscous matrix. Optical Materials. 27 , 1346, (2005).
10. R P, Mahajan, Ph. D. Thesis, Shivaji University, Kolhapur 2000.
11. I.H. Gul, Abbasi, A. Z , F. Amin, Anis-ur-Rehman, M., Maqsood, A., J. Magn. Magn. Matter.311, 494-499, (2007).
12. Rajeh kumar, Neeraj khare, Vijay kumar,and Bhalla, Applied Surface Scince, 7(2008) 254.
13. A.Beiser. Concepts of Modern physics. Mc Graw-Hill Kogakusha, LTD, 2ndedition 1980
14. Y.Sirotion and M. Shaskolskya, Fundamentals of Crystal. Physics",Mir Pub., Moscow1982.
15. NIRANJAN, SAHU, ''Study of crystal structure and electrical properties on lead titanate and lead zirconate titanate based ceramic oxids",Doctor of Philosophy,2011.
16. B. V. Hiremath, A. I Kingon, J.V. Biggers, J. Am. Ceram. Soc. 66 (1983) 790.
18. S. Kumar and R. Chandra: Temperature dependent studies of CdS nanoparticles in viscous matrix. Optical Materials. 27 , 1346, (2005).
21. Studies of pure and doped lead zirconate titanate ceramics and pulsed laser dfposited lead zirconate titanate thin films, M. PRABU,2013
22. I.H. Gul, A. Maqsood, Journal of Magnetism and Magnetic Materials 316 ,13-18. (2007).
23. A. M. M. Farea, Shalendra Kumar, Khalid Mujasam Batoo, Ali Yousef, Chan GyuLee, Alimuddin, J. Alloys Comp. 469 , 451-457, (2009).
24. S. Sindhu, M. R. Anathuraman, Bindu. P. Thampi, K. A. Malini and Philip Kuriam; Bull. Mater. Sci, 25, 599-607, (2000).